Fretting corrosion appears as reddish-brown (for steel) or black (for stainless) debris around the contact points of the wave crests. It is caused by small-amplitude oscillatory motion between the spring and the mating surface. This motion removes the protective oxide layer, leading to continuous oxidation and wear. In aerospace actuators, this can lead t...

Back to Q&A
Official Answer

Answer

Kwangirika kwangirika kugaragara nkumutuku-wijimye (ku byuma) cyangwa umukara (kubitagira umwanda) imyanda ikikije aho ihurira n’imiraba. Iterwa nigikorwa gito-amplitude oscillatory igenda hagati yisoko nubuso bwo guhuza. Iki cyerekezo gikuraho oxyde ikingira, biganisha kuri okiside ikomeza. Mu kirere cyo mu kirere, ibi birashobora kuganisha ku guterana. Umuti ni ukongera preload kugirango uhagarike urugendo cyangwa ugashyiraho isoko hamwe nigitambo cyangwa amavuta nka silver cyangwa Cadmium (aho byemewe).