Answer
Manyan karafan carbon kamar SAE 1070 zuwa 1090 suna da saurin kamuwa da sinadarin Hydrogen Embrittlement (HE) lokacin da aka yi amfani da acid pickling ko tsarin lantarki (misali, zinc ko nickel plating). Atomic hydrogen yana bazuwa cikin iyakokin hatsi, yana rage ƙarfin haɗin kai kuma yana haifar da gazawar ɓarna mai ɓarna ƙarƙashin nauyi mai tsayi. Don rage wannan, tsarin 'Baking' ya zama tilas. Dole ne a toya sassan a $190^{\circ}C \pm 10^{\circ}C$ na akalla sa'o'i 4 zuwa 24 (ya danganta da taurin da kauri) a cikin sa'o'i 1 zuwa 4 bayan plating. Don mahimmin sararin samaniya ko na'urorin mota, galvanizing na inji ko amfani da bakin karfe (wadanda ba su da kusanci ga HE) galibi ana fifita su don kawar da wannan yanayin gazawar gaba ɗaya.