Knowledge Answer

Ta yaya ƙimar ƙarfin aiki na austenitic bakin karafa ke tasiri ga murɗa maɓuɓɓugan ruwan raƙuman bakin ciki?

2026-06-16 FAQ

Bakin Karfe na Austenitic kamar 316 yana nuna babban ƙarfin aiki yayin jujjuyawar waya da tsarin murɗawa na gaba. Yayin da wayar ke siffata cikin bayanin martabar igiyar ruwa, nakasar filastik da aka keɓance tana ƙara ƙarfi da ƙarfi amma yana rage ductility. Don sassan bakin ciki sosai (misali, $t <0.005$ inci), kayan na iya zama britt...

Back to Q&A
Official Answer

Answer

Bakin Karfe na Austenitic kamar 316 yana nuna babban ƙarfin aiki yayin jujjuyawar waya da tsarin murɗawa na gaba. Yayin da wayar ke siffata cikin bayanin martabar igiyar ruwa, nakasar filastik da aka keɓance tana ƙara ƙarfi da ƙarfi amma yana rage ductility. Don sassa na bakin ciki sosai (misali, $t <0.005$ inci), kayan na iya zama tsinkewa, yana haifar da ƙananan fashewa a kololuwar kalaman. Sarrafa tsari ya ƙunshi sa ido kan kusurwar 'Springback' yayin murɗawa, wanda shine aikin rabon $E/E_{tan}$ (inda $E_{tan}$ shine modul ɗin tangent). Idan hardening aikin bai dace ba a cikin coil, sakamakon tsayin igiyoyin ruwa zai bambanta, wanda zai haifar da 'cocking' na bazara lokacin da ake lodi.

TOP