UNS: G10600-10900 DIN: 1.1231-1.1248 GB: C58D-C88D Modulus of elasticity: 206843 Recommended maximum operating temperature: 121 °C Main element chemical composition (wt%):C 0.55 - 0.88, Mn 0.40-0.90% Description and primary use: Common spring wire for bel
UNS: N05500 DIN: 2.4375 GB: 68Ni28Cu28Al Modulus of elasticity: 179140 Recommended maximum operating temperature: 287 °C Main element chemical composition (wt%):Ni 63.0 min%, Cu 27.0 -33.0%, Al 2.3 -3.1% Description and main use: with Monel 400 Have simil
UNS: N04400 DIN: 2.436 Elastic modulus: 179140 Recommended maximum operating temperature: 232°C Main element chemical composition (wt%) : Ni 63.0min %, Cu 28.0-34.0% Description and main uses: nickel-copper alloy spring wire has good corrosion resist
UNS: N10276 DIN: 2.4819 GB: NS3304 Elastic modulus: 211523 Recommended maximum operating temperature: 371°C Major element chemical composition (wt %) : 51.0 63.5% Ni, Cr 14.5 16.5%, 15.0 17.0% Mo, Fe 4.0 7.0% Description and main use: It has good co
UNS: N07718 DIN: 2.4668 GB: GH4169 Elastic modulus: 204085 Recommended maximum operating temperature: 704°C Main element chemical composition (wt%) : Ni 50.0-55.0%, Cr 17.0-21.0%, Fe11.0-24.0% Description and main use: Strength superior to inconel 6
UNS: N07750 DIN: 2.4669 GB: GH4145 Elastic modulus: 213737 Recommended maximum operating temperature: 371(538)°C Main element chemical composition (wt%) : Ni70.0min %, Cr 14.0-17.0%, Fe 5.0-9.0% Description and main use: nickel base precipitation ha
UNS: S66286 DIN: 1.498 GB: GH2132 Elastic modulus: 213737 Recommended maximum operating temperature: 538°C Major element chemical composition (wt %) : NI 24-27%, 13.5 16.0% Cr, Mo Ti 1.9 1.0-1.5% - 2.35%, V: 0.1 to 0.5% Description and main uses: Ir
UNS: S17700 DIN: 1.4568 GB: 07Crl7Ni7Al Elastic modulus: 203395 Recommended maximum operating temperature: 315°C Major element chemical composition (wt %) : Cr16.0-18.0%, 6.5 7.7% Ni, Al, 0.75 to 1.5% Description and main use: 300 series stainless s
UNS: S31600 DIN: 1.4401 GB: 06Crl7Ni12Mo2 Elastic modulus: 193053 Recommended maximum operating temperature: 204°C Major element chemical composition (wt %) : Cr: 16.5 18.0%, 10.5 13.5% Ni, Mo 2.0 2.5% Description and main uses: ordinary corrosion a
UNS: S30400 DIN: 1.4301 GB: 06Crl9Nil0 Elastic modulus: 193053 Recommended maximum operating temperature: 204°C Chemical composition of main elements (wt%) : Cr: 18.0-20.0%, Ni: 8.0-10.5% Description and main use: ordinary corrosion and heat resista